Automatic welding of the heads is performed with heating at a temperature of 120 to 250 degrees during seven days. The welding of the two welds required 660 kg of wire and 935 kg of flux.
Automatic welding of the heads is performed with heating at a temperature of 120 to 250 degrees during seven days. The welding of the two welds required 660 kg of wire and 935 kg of flux.